MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering N75L Nitrile Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Ultra-Low acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. To meet ASTM D2000/SAE J200 line call-out: MBF710, B34, F19.

Applications: Specifically formulated for use in pure air systems. The low acrylonitrile content of this compound provides excellent resistance to mineral oil, alcohol, paraffin and low-aromatic petrol in sub-zero temperature applications. Not recommended for use with acetone, benzene, chlorinated solvents or high-aromatic petrol. Good water resistance but poor against ozone and weather.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 70°IRHD; ASTM D1415
 73°IRHD, +3 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 10.8 MPa-10% change after 70 hours @ 100°C; ASTM D412
 12.0 MPaASTM D412
Elongation at Break 214.5 %-22% change after 70 hours @ 100°C; ASTM D412
 275 %ASTM D412
Compression Set 15 %
@Temperature 100 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 135 °C
Minimum Service Temperature, Air -60.0 °C
 -56.0 °CNon-brittle after 3 minutes
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Precision Polymer Engineering R60R Natural Rubber
Ensinger TECATRON™ GF 40 Polyphenylene sulfide (PPS)
Ensinger Tecamid® 6/6 Nylon (PA66)
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PPRECI198 / 57922

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.