MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Hytrel® RSR8847 BK209 TPC-ET  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 70 Shore A Low Hardness, High Performance Polyester Elastomer

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 12.1 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.5 MPaSpecimen type 5A; ISO 527-1/-2
Elongation at Break >= 300 %Specimen type 5A; ISO 527-1/-2
50% Modulus 2.80 MPa
@Strain 50 %
ISO 527-1/-2
100% Modulus 3.60 MPa
@Strain 100 %
ISO 527-1/-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 157 °C10°C/min; ISO 11357-1/-3
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 °CInjection, Optimum
Mold Temperature 30.0 °CInjection, Optimum
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
Dehumidified Dryer; Injection Molding; Injection
Moisture Content 0.080 %Injection
 
Descriptive Properties
Delivery formPellets
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking CodeTPC-ETISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationTPC-ETISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® HTR8341C BK320 TPC-ET
Celanese Hytrel® HTR8223 BK320 TPC-ET
DuPont Mobility and Materials Hytrel® HTR8341G BK320 TPC-ET
BASF Elastollan® 1185 A M TPUR
Celanese Hytrel® HTR8206 TPC-ET

PZDSY5236c / 239850

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.