Carbon black Chezacarb is manufactured by gasification of heavy petroleum residues by partial oxidation in Shell reactors. It is produced in the form of pellets of size 0,5 - 2,5 mm. Product is not classified as dangerous according to EC Directives. Carbon black Chezacarb is made in three sorts: A+, A and B. There are suitable mostly for modification of conductance and heat conductivity in plastics and rubber, due to their high specific surface and high poresity.Information provided by Unipetrol RPA |