MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton ARC 10 Paste grade machinable composite
Categories: Polymer; Thermoset; Epoxy

Material Notes: A reinforced composite for the repair and protection of metal surfaces. It is machinable with excellent compressive strength, chemical resistance and corrosion resistance. It is non-sagging, non-shrinking, and 100% solids. The ARC 10 is formulated for applications where machining to exact tolerances is required or desired. It is frequently used as an alternative to resurfacing by welding or flame spraying. ARC 10 is easily mixed and applied and cures without the need of heat or pressure.

Benefits:

  • High build characteristic allow for single coat applications
  • Tough resin structure resist thermal-mechanical shock
  • Outstanding adhesion insures reliable performance
  • Can be easily machined to exact tolerances
  • Convenient 4-1 mix ratio and verification of mix by color change
  • Performs well under fluctuating chemical environments
  • Resists compression setting.

Suggested Uses:

  • Condensers<>li>Cooling Water Pumps
  • Flange Faces
  • Hydraulic Rams
  • Keyways
  • Valve Bodies
  • Bearing Housings
  • Shafts
  • Spline Repairs
  • Pitted Castings
  • Heat Exchangers
  • Pump Volutes

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.00 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Hardness, Shore D 86ASTM D2240
Tensile Strength at Break 4000 psiASTM D638
Flexural Strength 10000 psiASTM D790
Flexural Modulus 510000 psiASTM D790
Compressive Strength 13000 psiASTM D695
Taber Abrasion, mg/1000 Cycles 275
@Load 0.250 kg
H-18/250g; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 66.0 °CWet
 93.0 °CDry
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 hour
@Temperature 32.0 °C
Light Load
 3.50 hour
@Temperature 25.0 °C
Light Load
 7.00 hour
@Temperature 16.0 °C
Light Load
 9.00 hour
@Temperature 10.0 °C
Light Load
 16.0 hour
@Temperature 32.0 °C
Full Load
 20.0 hour
@Temperature 25.0 °C
Full Load
 30.0 hour
@Temperature 32.0 °C
Full Chemical
 36.0 hour
@Temperature 16.0 °C
Full Load
 36.0 hour
@Temperature 25.0 °C
Full Chemical
 48.0 hour
@Temperature 10.0 °C
Full Load
 72.0 hour
@Temperature 16.0 °C
Full Chemical
 96.0 hour
@Temperature 10.0 °C
Full Chemical
Tack-Free Time 1.00 hour
@Temperature 32.0 °C
 2.00 hour
@Temperature 25.0 °C
 3.00 hour
@Temperature 16.0 °C
 5.00 hour
@Temperature 10.0 °C
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chesterton ARC S1HB Sprayable high-viscosity, 100% solids, advanced coating
3M Scotchkote™ HTX 517 Epoxy HT Lining
3M Scotchkote™ 162PWX Epoxy Coating
3M Scotchkote™ 162HB Epoxy Coating

PPTCHS046 / 138158

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.