MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NuSil VersaSil 60 MED-4062 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes:

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060
Tensile Strength at Break 9.00 MPa1310 psi
Tensile Stress at Strain  1.94 MPa
@Strain 100 %
282 psi
@Strain 100 %
 2.48 MPa
@Strain 300 %
360 psi
@Strain 300 %
 3.10 MPa
@Strain 200 %
450 psi
@Strain 200 %
Elongation at Break 875 %875 %
Tear Strength 43.8 kN/m250 pli
Compression Set 6.0 %6.0 %Method B
Tensile Set 16 %
@Strain 300 %
16 %
@Strain 300 %
 
Thermal PropertiesMetricEnglishComments
Shrinkage 2.6 %2.6 %
 
Processing PropertiesMetricEnglishComments
Working Life 642 min642 min
 
Descriptive Properties
ColorTranslucent
Plasticity85

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNUSIL479 / 142203

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.