MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lord Adhesives Chemlok® 6220 Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Chemlok® 6220 adhesive is a covercoat designed for use over Chemlok 205 primer. This adhesive system will bond a variety of uncured elastomers such as SBR, natural, nitrile and neoprene to metal substrates during the vulcanization of the elastomer. It is formulated without heavy metals and composed of a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in an organic solvent system.

Features: bonds a variety of elastomers and metals when used in combination with Chemlok 205 primer. provides excellent heat resistance at exposure temperatures as high as 149°C (300°F). provides superior resistance to heat and salt spray. formulated without heavy metals.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 - 0.995 g/cc0.0351 - 0.0359 lb/in³
Solids Content 25.5 - 29.5 %25.5 - 29.5 %by weight
Brookfield Viscosity 100 - 300 cP
@Temperature 25.0 °C,
Time 45.0 - 90.0 sec
100 - 300 cP
@Temperature 77.0 °F,
Time 0.0125 - 0.0250 hour
Brookfield LVT, Spindle 2, 30 rpm, Zahn Cup #2
 
Thermal PropertiesMetricEnglishComments
Flash Point 27.0 °C80.6 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9045 / 232434

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.