MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Novablend 6602 is a rigid, opaque PVC for molding compounds. This product has high impact, excellent indoor/outdoor weathering, high flow, and good processing characteristics.Applications includes: Electrical,Business machines,Telecommunications, Multi Purpose.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 8115 sec; ASTM D2240
Tensile Strength 45.5 MPaASTM D638
Elongation at Break 32 %ASTM D638
Tensile Modulus 2450 MPaType I; ASTM D638
Flexural Strength 70.3 MPaASTM D790
Flexural Modulus 2520 MPaASTM D790
Izod Impact, Notched 640 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 67.2 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 70.6 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 68.3 °C
@Thickness 3.18 mm
Annealed; ASTM D648
UL RTI, Electrical 105 °CUL 746
UL RTI, Mechanical with Impact 105 °Celong; UL 746
UL RTI, Mechanical without Impact 105 °CUL 746
Flammability, UL94 5VA
@Thickness 1.80 mm
All, Also UL 94 V-O @ 0.059 in thick.; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 199 - 204 °C
 
Descriptive Properties
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Outdoor Suitabilityf1UL 746C
Regional AvailabilityNorth America
UsesOutdoor Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding M5240 Polyvinyl Chloride, Rigid
Omnia Plastica PVC Polyvinylchloride
Bayshore Vinyl Compounds BRC R409006/HR.WHT Injection Molding Compound
Teknor Apex APEX® SRP 2700A Polyvinyl Chloride, Rigid
Chase Plastics CP Pryme® A100 ABS Molding Resin

PH0POL1428 / 145997

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.