MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Random Copolymer for Clear Storage Containers and Food and Beverage Containers

Formolene® 3355O is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for injection molding including thin wall applications requiring exceptionally good mold and part release. The use of an advanced clarifier with its aesthetic values, yellowness index and low haze, makes it an excellent choice for ‘see-through’ house wares and rigid packaging.

Formolene® 3355O meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact

Specimens were injection molded according to the conditions specified in ASTM D4101

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 55 g/10 min
@Temperature 230 °C
I2; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4200 psi2" (50mm) per min; ASTM D638
Elongation at Yield 14 %2" (50mm) per min; ASTM D638
Flexural Modulus, 1% Secant 150000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Temperature 23.0 °C
ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 185 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 15 %Plaque; FPC method
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene
Esenttia 45R60CD Random Copolymer Polypropylene
Flint Hills 23M2A Polypropylene Random Copolymer
Flint Hills 44S2A Polypropylene Impact Copolymer

PFPCPQ038 / 150270

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.