MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 65A NT0751 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne 65A NT0751 is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. 65A NT0751 resin offers high strength, rigidity and toughness over a broad range of demanding applications, and good fluid resistance to a wide variety of chemicals, solvents and oils.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 2.3 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 8.5 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50% RH; ISO 527-2
 55.0 MPaDAM; ISO 527-2
Tensile Strength, Yield 50.0 MPa50% RH; ISO 527-2
 85.0 MPaDAM; ISO 527-2
Elongation at Break 25 %DAM; ISO 527-2
 200 %50% RH; ISO 527-2
Elongation at Yield 5.5 %DAM; ISO 527-2
 21 %50% RH; ISO 527-2
Tensile Modulus 1800 MPa50% RH; ISO 527-2
 3100 MPaDAM; ISO 527-2
Flexural Strength 20.0 MPa50% RH; ISO 178
 75.0 MPaDAM; ISO 178
Flexural Modulus 700 MPa50% RH; ISO 178
 2800 MPaDAM; ISO 178
Poissons Ratio 0.40ISO 527-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 35.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 35.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °CUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CUnannealed; DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Zone 1 250 - 295 °CExtrusion
Zone 2 250 - 295 °CExtrusion
Zone 3 250 - 295 °CExtrusion
Zone 4 250 - 295 °CExtrusion
Zone 5 250 - 295 °CExtrusion
Die Temperature 270 - 295 °CExtrusion
Melt Temperature 270 - 295 °CExtrusion
 
Descriptive Properties
AdditiveHeat Stabilizer
Agency RatingsASTM, D4066 PA0123
 ASTM, D6779 PA0123
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
 FDA, 21 CFR 177.1500
 FED, L-P-410A
 MIL, M-20693B
AppearanceNatural Color
Automotive Material SpecificationStellantis 01378_20_03295
FeaturesChemical Resistant
 General Purpose
 Good Toughness
 High Rigidity
 High Strength
 Medium Viscosity
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9238 / 287594

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.