MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Samyang TRIEL® 5451GP Polyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Availability: Asia Pacific; Europe; North America

Form: Pellets

Information provided by Samyang Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ASTM D792
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.015 - 0.017 cm/cm0.015 - 0.017 in/inASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040ASTM D2240
Tensile Strength at Break 20.6 MPa2990 psiASTM D638
Tensile Stress  5.88 MPa
@Strain 5.0 %
853 psi
@Strain 5.0 %
ASTM D638
 8.34 MPa
@Strain 10 %
1210 psi
@Strain 10 %
ASTM D638
 12.8 MPa
@Strain 50 %
1850 psi
@Strain 50 %
ASTM D638
Elongation at Break >= 400 %>= 400 %ASTM D638
Flexural Yield Strength 5.39 MPa782 psiASTM D790
Flexural Modulus 0.0903 GPa13.1 ksiASTM D790
Izod Impact, Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
ASTM D4812
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 °C410 °FASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C163 °FUnannealed; ASTM D648
Vicat Softening Point 161 °C322 °FRate B (120°C/h), Loading 1 (10N); ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSAMY11373 / 312066

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.