MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos R08G-00 Random copolymer polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Film Grade

Material Notes: R08G-00 is a random copolymer polypropylene for film, blow molding, expanded PP foam beads, and injection molding applications with a barefoot additive package. This resin meets the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.

Information provided by INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.899 g/cc0.0325 lb/in³ASTM D792
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 7777ASTM D785
Tensile Strength at Break 24.8 MPa3600 psi2 in/min; ASTM D638
Tensile Strength, Yield 26.1 MPa3790 psi2 in/min; ASTM D638
Elongation at Break >= 900 %>= 900 %2 in/min; ASTM D638
Elongation at Yield 13 %13 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 848 MPa123000 psiASTM D790A
Izod Impact, Notched (ISO)  2.80 kJ/m²
@Temperature 4.00 °C
1.33 ft-lb/in²
@Temperature 39.2 °F
ASTM D256
 5.30 kJ/m²
@Temperature 23.0 °C
2.52 ft-lb/in²
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C174 °FASTM D648
Vicat Softening Point 132 °C270 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 60 %
@Thickness 1.30 mm
60 %
@Thickness 0.0512 in
Plaque. % diffuse transmittance; ASTM D1003
Gloss 92 %92 %@ 60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes21CFR 177.1520

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOS854 / 291460

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.