MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Equate EMDA-6147 HDPE Blow Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density provide excellent mold-ability, toughness and stress-cracking resistance. The molded articles exhibit good surface attributes.

Applications: EMDA-6147 is suitable for blow molding of closed head shipping containers of up to 50 liter size, fuel tanks, drums, jerry cans and other similar parts. The molded parts have smooth surfaces that can be readily treated for high quality printing. The containers may be utilized for packaging a variety of aggressive materials such as industrial chemicals, latex paint, printing inks and adhesives. Food can also be packaged in the containers in line with conformity of the resin with food contact regulations. EMDA-6147 is also suitable for making non-pressure “gravity” pipes for drainage and sewage applications

Information provided by Equate

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D792
ESCR 100% Igepal® 1000 hour
@Temperature 50.0 °C
ASTM D1693 B
Melt Flow 0.070 g/10 min
@Load 2.16 kg
ASTM D1238
High Load Melt Index 9.0 g/10 min
@Load 21.6 kg
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 35.0 MPaASTM D638
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Break >= 750 %ASTM D638
Flexural Modulus 1180 MPaASTM D790
Izod Impact, Unnotched (ISO) 17.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 131 °CEquate Test Method
Crystallization Temperature 116 °CEquate Test Method
Vicat Softening Point 125 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 204 °C
Zone 2 204 °C
Zone 3 204 °C
Zone 4 204 °C
Die Temperature 204 °C
Melt Temperature 210 °C
Head Temperature 204 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Global B-8200 High Density Polyethylene
Chevron Phillips Marlex® HHM 5502 BZ High Density Ethylene Hexene Copolymer
Chevron Phillips Marlex® C513UV HDPE Blow Molding Resin
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
Global B-5200 High Density Polyethylene

PEQUAT901 / 150429

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.