MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LNP Lubricomp® DL-4030 Polycarbonate, PTFE Additive  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, PTFE Filled

Material Notes:
  • Features: Lubricated
  • Forms: Pellets
  • Processing Method: Injection Molding

Information provided by LNP, a GE Plastics Company.

This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.28 g/ccMethod A; ASTM D792
Density 1.28 g/ccISO 1183
Water Absorption 0.10 %at 24 hrs; ASTM D570
Linear Mold Shrinkage 0.0080 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0080 - 0.0090 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.6 MPaASTM D638
Tensile Strength, Yield 51.7 MPaASTM D638
Elongation at Break 38 %ASTM D638
Elongation at Yield 6.1 %ASTM D638
Tensile Modulus 2.07 GPaASTM D638
Flexural Strength 75.8 MPaASTM D790
Flexural Modulus 2.19 GPaASTM D790
Izod Impact, Notched 2.72 J/cm
@Thickness 3.18 mm
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.18 mm
ASTM D256
Izod Impact, Notched (ISO) 28.5 kJ/m²ISO 180
Izod Impact, Unnotched (ISO) 137 kJ/m²ISO 180
Falling Dart Impact 30.6 JASTM D3763
Instrumented Impact Total Energy 34.1 JMulti-Axial Instrumented Impact Energy; ISO 6603-2
Coefficient of Friction, Dynamic 0.25vs. Steel - @ 40 psi, 50 ft/min, tested in accordance with LNP WI-0687; ASTM D1894
Coefficient of Friction, Static 0.12vs. Steel @ 40 psi, in accordance with LNP WI-0687; ASTM D1894
K (wear) Factor 36.0 x 10-10 in³-min/ft-lb-hr40psi, 50ft/min; tested in accordance with LNP WI-0687
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 128 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 299 - 316 °C
Mold Temperature 79.4 - 107 °C
Drying Temperature 121 °C
Dry Time 4 hour
Moisture Content 0.020 %Suggested
Back Pressure 0.172 - 0.345 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LNP Lubricomp® DL-4020 Polycarbonate, PTFE Additive
LNP Stat-Kon® D- FR ECO Polycarbonate, Carbon Powder
RTP Company RTP 399 X 113385 B Polycarbonate (PC); LDS Platable
LNP Lubricomp® DCL-4036 Polycarbonate, Carbon Fiber Reinforced, PTFE Lubricant
LNP Lubricomp® RL-4030 BK8-115 Polyamide 66, PTFE Additive

PZLNP1136 / 51218

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.