MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP1325LV Thixotropic, Heat Curing Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP1325 and EP1325LV are one part thixotropic, heat curing epoxy adhesives. They can also be used as a small mass potting compounds, staking or damming adhesives, or polymer systems where the application requires low shrinkage and excellent adhesion to a wide variety of plastics, metals and circuit board materials. These products give very good environmental protection and dielectric properties over a wide temperature range. The primary difference between the two versions is the LV version has a lower high shear viscosity (higher press flow rate) to provide easier dispensing. The amount of sag upon curing is the same.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccTM R050-16
Water Absorption 0.11 %
@Time 86400 sec
TM R050-35
Viscosity 250000 cPRVT, #7, 2.5 rpm; TM R050-12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85TM R050-17
Tensile Strength at Break 6500 psiTM R050-36
Tensile Strength, Ultimate 6500 psiTM R050-36
Tensile Strength, Yield 5000 psiTM R050-36
Elongation at Break 0.00 - 1.0 %TM R050-36
Tensile Modulus 700 ksiTM R050-36
Compressive Yield Strength 13000 psiTM R050-38
Compressive Strength 14000 psiBreak; TM R050-38
 17000 psiUltimate; TM R050-38
Compressive Modulus 600 ksiTM R050-38
Adhesive Bond Strength 1800 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+14 ohm-cm
Dielectric Constant 3.5
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 440 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°C
Thermal Conductivity 0.360 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 97.0 °CTM R050-25
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 10.0 min
@Temperature 150 °C
 15.0 min
@Temperature 120 °C
 30.0 min
@Temperature 110 °C
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESL141 / 101555

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.