MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite Durez® 29781 Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez 29781 is a finely pulverized two-step phenolic resin. Durez 29781 is recommended for use in the manufacture of dry mix truck blocks and disc brake pads. Durez 29781 contributes good friction and fade resistance to formulations.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 200 Mesh200 MeshScreen Percent: < 1.0; DCT 4007A
 
Thermal PropertiesMetricEnglishComments
Softening Point 80.0 °C176 °Fcap. Shrink; DCT 4000B
 
Processing PropertiesMetricEnglishComments
Cure Time 0.500 min
@Treatment Temp. 165 °C
0.00833 hour
@Treatment Temp. 329 °F
DCT 0162B
 
Descriptive Properties
% Hexamine Content8.5DCT 4019A
Inclined Plate Flow; 0.2g, 125°C, mm40DCT 4009B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Bakelite® PF 7595 Phenolic Formaldehyde Resin, Low Coefficient of Friction, Galvanized, Conductive
Bakelite® MP 4165 Melamine Phenolic Resin, Copper Adhesive, Low Shrinkage, High Mechanical Strength
Sumitomo Bakelite Durez® 33160 Phenolic Resin
Sumitomo Bakelite Durez® 13037 Phenolic Resin

PSUMIT239 / 194044

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.