Purell RP271G is a low melt flow polypropylene random copolymer resin with good clarity, good impact properties, high temperature resistance suitable for autoclave sterilization. Typical customer application are medical IV solution bottles made by extrusion blow molding process. Applications: Bottles For Consumer Goods, Healthcare Applications .Information provided by LyondellBasell. |