MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Mobility and Materials Minlon® 12T NC010 PA66-IMD36  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Mineral Filled

Material Notes: 36% Mineral Reinforced, Toughened, Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³DAM; ISO 1183
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
DAM; Sim. to ISO 62
 6.2 %
@Thickness 2.00 mm
6.2 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
1.70 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 58.0 MPa8410 psi50% RH; ISO 527-1/-2
 80.0 MPa11600 psiDAM; ISO 527-1/-2
Elongation at Break 18 %18 %DAM; ISO 527-1/-2
 40 %40 %50% RH; ISO 527-1/-2
Tensile Modulus 2.00 GPa290 ksi50% RH; ISO 527-1/-2
 4.90 GPa711 ksiDAM; ISO 527-1/-2
Flexural Modulus 1.80 GPa261 ksi50% RH; ISO 178
 4.50 GPa653 ksiDAM; ISO 178
Poissons Ratio 0.350.35DAM; ISO 527-1/-2
 0.400.4050%RH; ISO 527-1/-2
Izod Impact, Notched (ISO)  90.0 kJ/m²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1U
 100 kJ/m²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1U
 190 kJ/m²
@Temperature 23.0 °C
90.4 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1U
 330 kJ/m²
@Temperature 23.0 °C
157 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1U
Izod Impact, Unnotched (ISO)  5.00 kJ/m²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 5.00 kJ/m²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 9.00 kJ/m²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 12.0 J/cm²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 21.0 J/cm²
@Temperature 23.0 °C
99.9 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 33.0 J/cm²
@Temperature 23.0 °C
157 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 0.400 J/cm²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.50 J/cm²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; IEC 62631-3-1
Dielectric Constant  3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
DAM; IEC 62631-2-1
Dielectric Strength 24.0 kV/mm610 kV/inDAM; IEC 60243-1
Dissipation Factor  0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.010
@Frequency 100 Hz
0.010
@Frequency 100 Hz
DAM; IEC 62631-2-1
Comparative Tracking Index 400 V400 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 64.0 µm/m-°C35.6 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C36.1 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 256 °C493 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FDAM; ISO 75-1/-2
Flammability, UL94  HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
<= 3.15 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 25 %25 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 - 305 °C545 - 581 °FInjection
 295 °C563 °FInjection Optimum
Mold Temperature 70.0 - 120 °C158 - 248 °FInjection
 100 °C212 °FInjection Optimum
Ejection Temperature 210 °C410 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)3Injection
Max. screw tangential speed (m/s)0.2Injection
Part Marking CodePA66-IMD36ISO 11469
ProcessingInjection Molding
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66-IMD36ISO 1043
Special characteristicsHeat stabilized or stable to heat

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Minlon® 11C40 NC010 PA66-IMD40
A. Schulman Diamond Centrex® 821 ASA Weatherable Polymers Injection Molding Grade
DuPont Mobility and Materials Minlon® 12TA BKB124 PA66-IMD32
Crystex Composites Mykroy/Mycalex MM 501 Molding Grade Glass-bonded Mica Composite
Colorite Polymers Self Frosting™ 9511SF Vinyl Compound

PDSX5245 / 197885

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.