MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addolink® R PU Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Information: Product information Addolink R gives shorter casting and demolding times than Addolink B. It is used particularly in the production of soft hot-curing cast elastomers whose casting times would be too long if Addolink B were used. The accelerating effect of Addolink R is so strong, however, that this product is always mixed with Addolink B, with which it is miscible at all ratios. The most suitable Addolink R / Addolink B ratio for the system in question should be determined in advance.

Function: Crosslinking agent for the production of polyurethane elastomers (hot-curing cast systems).

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.02 g/cc0.0368 lb/in³
Water Absorption <= 0.20 %<= 0.20 %
Viscosity 72 cP72 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point 18.0 °C64.4 °FFreezing Point
Flash Point 135 °C275 °FASTM D93, DIN EN 22719
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearanceclear, colorless liquid
Hydroxyl value1245 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyurethane, Liquid
Lanxess Urepan® 600 Polyurethane Rubber

PLANY8211 / 208604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.