MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei TENAC™-C NS556 Copolymer Acetal (POM), Medium Viscosity, Mineral Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Excellent balance of mechanical properties, low friction and wear characteristics. Applications: Automotive parts, electrical & electronic parts, industrial parts.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cmAsahi Kasei
Melt Flow 9.0 g/10 minISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.0 MPa50% RH; ISO 527
Elongation at Break 25 %50% RH; ISO 527
Tensile Modulus 4300 MPa50% RH; ISO 527
Flexural Modulus 4100 MPa50% RH; ISO 178
Charpy Impact, Notched 6.00 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 100 µm/m-°CISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 124 °CISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei TENAC™-C G4555 Copolymer Acetal (POM), Medium Viscosity, GF Reinforced
Asahi Kasei TENAC™-C CF452 Copolymer Acetal (POM), Medium Viscosity, Carbon Fiber Reinforced
Asahi Kasei TENAC™-C 3513 Copolymer Acetal (POM), High viscosity
Asahi Kasei TENAC™-C G4575 Copolymer Acetal (POM), Medium Viscosity, GF Reinforced
BASF Ultraform® N 2640 Z2 UNC Q600 POM

PASAHI8099 / 221126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.