MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Schott PCE Photofilter Red 625
Categories: Ceramic; Glass; Optical; Filter

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.57 g/cc0.0928 lb/in³
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 µm/m-°C
@Temperature 20.0 - 300 °C
5.00 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 519 °C966 °F
Softening Point 725 °C1340 °Fη=7.67.6 dPas
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5121.512
Transmission, Visible 5.3 %5.3 %VD65
 5.6 %5.6 %VC
 9.8 %9.8 %VA
 0.00 %
@Thickness 2.00 mm,
Wavelength 580 nm
0.00 %
@Thickness 0.0787 in,
Wavelength 580 nm
 1.0 %
@Thickness 2.00 mm,
Wavelength 600 nm
1.0 %
@Thickness 0.0787 in,
Wavelength 600 nm
 25 %
@Thickness 2.00 mm,
Wavelength 620 nm
25 %
@Thickness 0.0787 in,
Wavelength 620 nm
 82 %
@Thickness 2.00 mm,
Wavelength 640 nm
82 %
@Thickness 0.0787 in,
Wavelength 640 nm
 91 %
@Thickness 2.00 mm,
Wavelength 660 nm
91 %
@Thickness 0.0787 in,
Wavelength 660 nm
 92 %
@Thickness 2.00 mm,
Wavelength 680 nm
92 %
@Thickness 0.0787 in,
Wavelength 680 nm
 
Descriptive Properties
Colorimetry0.286A, y
 0.287C, y
 0.288D65, y
 0.712D65, x
 0.713C, x
 0.714A, x
Edge wavelengths620-630 nm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGT9887 / 183140

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.