Copolymer with low emission, without halogen and antimony oxide. Natural and colored PP based compound. U.L. approved for automotive, electrical, appliances, tools, and other industrial parts. These compounds are used mainly in the automotive and household industry to manufacture outer casings and protection guards, in the furniture sector to manufacture chairs, for the production of footwear, and for the production of sport articles such as helmets, ski boots, and roller blades. Information provided by SO.F.TER. Spa |