MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schweitzer-Mauduit Argotec™ 46510 Uncoated high performance aliphatic thermoplastic polyurethane (TPU) film
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Argotec™ 46510 is an uncoated high performance aliphatic thermoplastic polyurethane (TPU) film designed for a variety of paint, metal and surface protections. These applications include automotive OEM and aftermarket. Argotec 46510 films are ideal for protection with excellent UV resistance, superior durability, and consistent optical clarity with a high gloss finish. The increased hardness of Argotec 46510 provides enhanced stain resistance as compared to other standard paint protection films.

Attributes: Maintain surface appearance with UV and enhanced stain resistance (non-yellowing). Longevity from highly durable, self-healing, scratch and chip resistance. Superior appearance with paint like gloss finish. Operational efficiency during coating process from superior film gauge and gel control. Customized to end application with variety of width and gauge options. Local manufacturing capabilities for just in time delivery.

Information provided by Schweitzer-Mauduit International, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 127 - 305 microns5.00 - 12.0 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D-2240
Tensile Strength, Ultimate 64.8 MPa9400 psiASTM D-412
Elongation, Ultimate 370 %370 %ASTM D-412
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 90 %90 %@ 60°; ASTM D523
Transmission, Visible 93 %93 %ASTM D1003
 
Descriptive Properties
Accelerated Aging QUVA< 2.0 delta YI up to 2500 hours340 nm
LengthUp to 22"Outside diameter
Width49" -51"
 56" - 62"

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSCHWE908 / 287669

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.