MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Chemical Industry KAIFA® 301-G0F PBT Resin
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Flame Retardant

Material Notes: Flame retardant, good flow, low bleeding

Information provided by Beijing Chemical Industry Research Institute (Group)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
Water Absorption 0.090 %24 hr; ASTM D570
Linear Mold Shrinkage 0.015 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaASTM D638
Elongation at Break 80 %ASTM D638
Flexural Strength 100 MPaASTM D790
Flexural Modulus 2.40 GPaASTM D790
Charpy Impact Unnotched 4.50 J/cm²ISO179
Charpy Impact, Notched 0.500 J/cm²ISO179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 22.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 250 V
@Thickness 3.20 mm
ASTM D3638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 170 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 225 - 255 °C
Nozzle Temperature 245 °C
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 130 °C
Dry Time 4 hour
Injection Pressure 80.0 - 120 MPa
Back Pressure 8.00 - 18.0 MPa
Screw Speed <= 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKAIF18 / 48600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.