MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt HUP 17/25 RB-Colour Sheet Molding Compound Fire Retardancy
Categories: Polymer; Thermoset

Material Notes:

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccISO 1183 A
Filler Content 25 %ISO 1172
Water Absorption <= 0.30 %ISO 62
Linear Mold Shrinkage 0.0010 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 MPaISO 527-4
Flexural Strength 150 MPaISO 14125
Flexural Modulus 9500 MPaISO 14125
Tensile Impact Strength 65.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 4.5
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 22.0 kV/mmIEC 60243-2-1
Dielectric Loss Index 0.020
@Frequency 1000 Hz
tan s; IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-2
Flammability, UL94 V-0
@Thickness 3.50 mm
Glow Wire Flammability Index 960 °C
@Thickness >=2.00 mm
IEC 60695-2-1
 960 °C
@Thickness >=2.55 mm
punched plate; IEC 60695-2-1
 
Processing PropertiesOriginal ValueComments
Mold Temperature 140 - 150 °C
Hold Pressure 1160 - 1740 psiMolding pressure
Cure Time 65.0 secISO 12114/1
 
Descriptive Properties
Fiber length25 mmPA3.01
Molding time>25 s/mm
Surface Weight4000 g/m2ISO 10352

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9118 / 231713

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.