MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shuman 730 Utility White ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.

Data provided by the Shuman Plastics, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Melt Flow 2.0 - 6.0 g/10 min2.0 - 6.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 102102ASTM D785
Izod Impact, Notched 2.14 J/cm4.00 ft-lb/in1/8 in sample; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C169 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 216 °C350 - 420 °FExtrusion
 204 - 227 °C400 - 440 °FInjection
Drying Temperature 76.7 - 93.3 °C170 - 200 °F4 to 24 hrs; Tray Dryer
 87.8 - 93.3 °C190 - 200 °F2 to 24 hrs; Dehumidifying Dryer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® X AS/018 White Acrylonitrile Butadiene Styrene (ABS)
Westlake Plastics Absylux® FR Acrylonitrile-Butadiene-Styrene Flame Retardant
Shuman 330 White PC/ABS Alloy
Multibase Multi-ABS 802 Utility Grade White
Multibase Multi-ABS 1030 White

PSHU03A / 67535

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.