MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Persian Gulf Polymer HDPE - HBYL1 (Yellow) Recycled Blow Molding Grade
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: A post-consumer high density polyethylene (HDPE - HBYL1) offers an excellent combination of toughness, load bearing strength and process ability characteristics. It is classified as a multipurpose blow molding grade. It may be blow molded into containers for household and industrial chemicals (e.g. detergents, bleach, fabric softeners, solvents, paints, etc.), automotive supplies, toiletries and cosmetics. It can also be used in other hollow thin-walled parts and profile extrusions.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ASTM D792
Melt Flow 0.32 g/10 min
@Load 10.0 kg,
Temperature 220 °C
0.32 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7979ASTM D2240
Tensile Strength at Break 38.0 MPa5510 psiASTM D638
Tensile Strength, Yield 43.0 MPa6240 psiASTM D638
Modulus of Elasticity 4.30 GPa624 ksiASTM D638
Flexural Yield Strength 60.2 MPa8730 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPERSI989 / 250393

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.