MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Tra-Con Tra-Bond FDA2T Food and Drug Application Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND FDA-2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval. This two-part amber adhesive is easily mixed, used and cured at room temperature for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND FDA-2T is an effective electrical insulator, and it provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 26000 cP26000 cPMixed (rv #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8080
Elongation at Yield 9.0 %9.0 %
Adhesive Bond Strength 12.4 MPa1800 psiLap shear, alum to alum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+14 ohm-cm1.20e+14 ohm-cm
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm420 kV/in
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 53.0 µm/m-°C
@Temperature 20.0 °C
29.4 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 145 °C293 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 70.0 °C158 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
USP Class VI YesYes
 
Descriptive Properties
Color Hazy, Amber
Mix Ratio, parts by weight100/93Resin/Hardener
Working Life hours 3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC265 / 71193

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.