MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® FG1901 G (SEBS) grafted with MA
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form identified:
FG1901 GT - supplied as a dusted pellet

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton FG1901 G is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; and Impact Modification

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D792
Viscosity 5000 cPBAM 922
Melt Flow 14 - 28 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 71
@Time 10.0 sec
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 34.5 MPaTypical properties of film cast from toluene solution; ASTM D412
Elongation at Break 500 %Typical properties of film cast from toluene solution; ASTM D412
 
Descriptive Properties
ContentMaleic anhydride1.4-2.0%, BAM 1026
Styrene/Rubber Ratio30/70
Water<500 ppmwat time of packaging, BAM 1024

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® G1701 M (SEP) Linear Diblock Copolymer
Kraton® G1654 H (SEBS) Linear Triblock Copolymer
Kraton® G1641 H (SEBS) Linear Triblock Copolymer
Kraton® G1651 E (SEBS) Linear Triblock Copolymer
Kraton® G7820 GU-N (SEBS) Compound

PKRA9920 / 132820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.