MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® 101L BKB009 PA66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Unreinforced Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50% RH; ISO 527-1/-2
 88.0 MPaDAM; ISO 527-1/-2
Elongation at Break 16 %DAM; ISO 527-1/-2
 >= 50 %50% RH; ISO 527-1/-2
Elongation at Yield 4.6 %DAM; ISO 527-1/-2
 25 %50% RH; ISO 527-1/-2
Tensile Modulus 1400 MPa50% RH; ISO 527-1/-2
 3050 MPaDAM; ISO 527-1/-2
Flexural Modulus 1200 MPa50% RH; ISO 178
 2800 MPaDAM; ISO 178
Poissons Ratio 0.37DAM; ISO 527-1/-2
 0.4350%RH; ISO 527-1/-2
Charpy Impact Unnotched 134 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 203 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 3.70 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 4.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 262 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 190 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CDAM; ISO 75-1/-2
Flammability, UL94 V-2
@Thickness 0.710 mm
DAM; IEC 60695-11-10
 V-2
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 300 °CInjection
 290 °CInjection Optimum
Mold Temperature 50.0 - 90.0 °CInjection
 70.0 °CInjection Optimum
Ejection Temperature 190 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %Injection
Hold Pressure 50.0 - 100 MPaInjection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds5 µgC/gVDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging F-value (refraction) (%)99ISO 6452; DAM
Fogging G-value (condensate) (mg)0.1ISO 6452; DAM
Hold pressure time (s/mm)4Injection
Max. screw tangential speed (m/s)0.4Injection
Odor3VDA 270
Part Marking CodePA66ISO 11469
ProcessingInjection Molding
Regional AvailabilityNorth America
 South and Central America
Resin IdentificationPA66ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 101 NC010 PA66
Celanese Zytel® 101L BKB080 PA66
Celanese Zytel® 101F BKB009 PA66
Celanese Zytel® 101L NC010 PA66
BASF Ultradur® B 4520 PBT

PDSX5295 / 197935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.