Low aging, superior coupling, high dielectric constant, and the high charge constant. Used for hydrophones, receivers, low power projectors, and in micropositioning devices.Data provided by Harris Acoustic Sensors. Harris Acoustic Sensors has acquired EDO Ceramics. This grade is available from Harris. |