MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
PolyMirae Adstif HA748L Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Adstif HA748L is a high crystallinity polypropylene homopolymer, which features an extremely high stiffness, high gloss and maintaining mechanical properties even at high temperatures. Adstif HA748L is selected by customers for use in the production of stiff injection moulded articles where high rigidity is needed. Typical applications of HP748L include food packaging containers, housewares, small appliances and technical parts. It is typically used by customers in small appliances and automotive compounding applications where high rigidity and very good thermal characteristics are required. Adstif HA748L is used in food contact.

Product Features: Very high long term heat resistance and High HDT/ High Stiffness/High Crystallization Temperature/High surface hardness/ Good pigment dispersion/UL94 HB Class and cUL/Relative thermal Index (RTI) : Project Opening by UL Korea

Typical Applications: Small appliances and technical parts/Rice cooker case/Microwave oven/Electric Kettle /Auto compound/Heater case/Food packaging containers/Housewares

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D1505
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ASTM D785
Tensile Strength, Yield 400 kg(f)/cm²ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 22500 kg(f)/cm²ASTM D790
Izod Impact, Notched 14.5 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 130 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PolyMirae Adstif EA640G High stiffness sheet Polypropylene Copolymer
Aclo Accucomp Polypropylene HPO306L Homopolymer
Braskem H 502HC Thermoforming Polypropylene Homopolymer
LyondellBasell Adstif HA 5029 Polypropylene
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride

PMIRAF36 / 183257

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.