MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Solvay VTM® 264S-1 Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: VTM264-1 & VTM264S-1 resin systems are toughened, 65 to 120°C (149 to 248°F) curing temperature epoxy resin matrices specifically developed for oven vacuum bag processing of large structures. The resins are particularly suited to the marine and industrial markets.

Features & Benefits:

  • Outstanding vacuum only processing capability on a wide range of reinforcements
  • Flexible curing capability
  • Up to 30 days out life 12°C (70°F)
  • 12 months storage at -18°C (0°F)
  • Service temperature up to 100°C (212°F)
  • VTM264-1 made via holt melt process
  • VTM264S-1 made via solvent impregnation process
  • Suitable for component and tooling manufacture
  • Fully co-curable with the VTM260 range of adhesives, surfacing films and syntactic plies

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc1 hr at 120°C
Storage Temperature -18.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Glass Transition Temp, Tg 81.0 °CDMA E' 16 hrs at 65°C+1 hr at 120°C, wet
 83.0 °CDMA E' 16 hrs at 65°C
 102 °CDMA E' 5 hrs at 80°C
 114 °CDMA E' 16 hrs at 65°C+1 hr at 120°C, dry
 114 °CDMA E' 5 hrs at 80°C+1 hr at 120°C, dry
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 120 °C
 2.00 hour
@Temperature 100 °C
 5.00 hour
@Temperature 80.0 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCYTED164 / 180466

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.