MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Unoba® EP NLGI Grade 0
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Unoba EP is a multipurpose, extreme-pressure lithium grease developed for use in a wide variety of industrial and automotive applications. It is a versatile, general-purpose grease for use in applications where operating temperatures and loads are moderate. Unoba EP is manufactured with high-quality base oils thickened with lithium 12-hydroxystearate soap. It is fortified with extreme pressure and antiwear additives plus rust and oxidation inhibitors. It has good load-carrying capacity for protection against wear, good oxidation resistance for long service life, protects metal parts against rust and corrosion, and is resistant to water washout. It has good resistance to structural breakdown and will not soften excessively during high-speed operation in rolling-element bearings. It forms a good seal to help minimize bearing contamination. Unoba EP is available in multiple grades for use in a wide variety of applications. It is an excellent grease for use in centralized lube systems. The semifluid grades may be used in enclosed industrial gearboxes where oil leakage is a problem.

Applications:

  • Plain and rolling-element bearings in compressors, fans, centrifugal pumps and other industrial equipment where operating temperatures and loads are moderate
  • Chassis parts, universal joints and water pumps on passenger cars, light trucks and other mobile equipment
  • Track rollers, commercial lawn mowers, crushers and vibrating screens (semifluid grades)
  • Enclosed gear drives on industrial, mining and mobile equipment where oil leakage is a problem (semifluid grades)
  • Wheel bearings of passenger cars equipped with drum brakes
  • Centralized grease lubrication systems
  • General-purpose shop/industrial grease
Features/Benefits:
  • Multipurpose grease for use in a wide variety of applications
  • Good extreme-pressure and antiwear properties
  • Good shear stability
  • Good oxidation resistance and thermal stability
  • Resists water washout
  • Suitable for use in centralized lube systems

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.886 g/cc0.0320 lb/in³
Viscosity Measurement 8181Index
Saybolt Viscosity at 100°F 750 SUS750 SUS
Saybolt Viscosity at 210°F 72 SUS72 SUS
Kinematic Viscosity at 40°C (104°F) 142 cSt142 cSt
Kinematic Viscosity at 100°C (212°F) 13 cSt13 cSt
Oxidative Stability 100 hour
@Pressure 0.0345 MPa
100 hour
@Pressure 5.00 psi
Pressure Drop; ASTM D942
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)ASTM D2596
Four Ball Wear 0.450 mm0.0177 inScar Diameter; ASTM D2266
Penetration P(60), 1/10 mm 355 - 385355 - 385ASTM D217
Timken Test 22700 g50.0 lbASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 107 °C225 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Dropping Point >= 172 °C>= 342 °F
 
Descriptive Properties
ColorGreen
ThickenerLithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5154 / 198407

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.