MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECATEC PPS CF50 CP/IP/OS S0001 natural - Polyphenylene Sulfide, Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler

Material Notes: Fillers: carbon fibers

Main features:

  • excellent chemical resistance
  • inherent flame resistance
  • excellent mechanical properties
  • continuous service temperature up to 150 °C
Target Industries:
  • automotive industry
  • mechanical engineering
  • oil and gas industry
  • safety engineering
  • sporting goods

Information provided by Ensinger Composites.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.52 g/cc
Filler Content 50.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 680 MPaISO 527-4
Tensile Modulus 55.0 GPaISO 527-4
Flexural Strength 780 MPaISO 14125
Flexural Modulus 57.0 GPaISO 14125
Compressive Strength 650 MPaISO 14126
Compressive Modulus 51.0 GPaISO 14126
Shear Strength 131 MPainterplanar; ISO 14129
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°Cin 0° and 90° direction
Melting Point 285 °C
Maximum Service Temperature, Air 230 °Clong term
 260 °Cshort term
Glass Transition Temp, Tg 60.0 °C
 
Processing PropertiesOriginal ValueComments
Drying Temperature 150 °C
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Areal weight finished product349 g/m²
Colornatural
Fiber architectureTwill 2/2
Fiber areal weight200 g/m²
Fiber typeCarbon HT 3k
Material widths1000 mm
 1270 mm
ply thickness (consolidated)0.2 mm
Resin weight content0.427

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN515 / 287739

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.