MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling SUSTAMID® 66 PA 66/Extruded Nylon
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:
  • Good dimensional stability
  • Very good sliding properties
  • High abrasion resistance
Product applications:
  • Mechanical engineering
  • Aircraft construction
  • Electrical industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 8.5 %8.5 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Hardness, Rockwell R 121121ASTM D785
Hardness, Shore D 8080ASTM D2240
Tensile Strength, Yield 82.7 MPa12000 psiASTM D638
Elongation at Break 40 %40 %ASTM D638
Tensile Modulus 2.76 GPa400 ksiASTM D638
Flexural Strength 103 MPa15000 psiASTM D790
Flexural Modulus 2.90 GPa420 ksiASTM D790
Compressive Strength 86.2 MPa12500 psiASTM D695
Shear Strength 68.9 MPa10000 psiASTM D732
Izod Impact, Notched 0.320 J/cm0.600 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.250.25
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+13 ohm>= 1.00e+13 ohmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 13.8 kV/mm351 kV/inASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 81.0 µm/m-°C45.0 µin/in-°FASTM D696
Thermal Conductivity 0.245 W/m-K1.70 BTU-in/hr-ft²-°F
Melting Point 260 °C500 °FASTM D3418
Maximum Service Temperature, Air 104 °C220 °F
Deflection Temperature at 0.46 MPa (66 psi) 199 °C390 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C195 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ 101 / Ertalon™ 66 SA PA66 Extruded, Unfilled, Type 66 Natural and Black
EPICHEM PA 66 Polyamide 66
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
EPICHEM Epinyl PA 66 Polyamide 66
Domo TECHNYL® A 218 V30 Black 21 NS PA 66 30% Glass Reinforced, Conditioned

PROCH9036 / 232739

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.