MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

DuPont Styrofoam™ Polystyrene Rigid Foam Insulation
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: The information below is typical of Styrofoam™ rigid polystyrene foam used for construction insulation - but many specific grades are available. This material is produced as sheets of closed-cell foam by a continuous extrusion process. Its properties will be different than expanded polystyrene beads because beads have voids between cell walls. Styrofoam is a trademark of Dow Chemical.

This former Dow product line is now a DuPont product line.

Key Words: Compare to Expanded Polystyrene (EPS)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0350 g/cc0.00126 lb/in³
Water Absorption 9.0 %9.0 %about 9% by weight or 0.3% by volume.
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 0.500 MPa72.5 psiVaries with grade. A safety factor of three is recommended for long term static load or traffic use.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.0270 W/m-K0.187 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 75.0 °C167 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Styrofoam™ SM Extruded Polystyrene Foam Insulation
DuPont Styrofoam™ Scoreboard Extruded Polystyrene Foam Insulation
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
DuPont Styrofoam™ Ultra SL Extruded Polystyrene Foam Insulation
Overview of materials for Nylon 12

PDWZ00 / 34650

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.