MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake ELEVATE® EF546 Ethylene Vinyl Acetate Copolymer
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: ELEVATE® EF546 is a 6% vinyl acetate copolymer designed for general purpose packaging films. This resin has excellent clarity, toughness, heat sealing characteristics, low temperature brittleness properties, and machine ability.

Test specimens for blown film: nominal thickness 1.25 mils; blow up ratio 2.5:1, die gap 35 mils at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D1505
Melt Index of Compound 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 440 %440 %ASTM D882
Film Elongation at Break, TD 770 %770 %ASTM D882
Dart Drop 6.30 g/micron160 g/milASTM D1709A
Film Tensile Strength at Break, MD 31.0 MPa4500 psiASTM D882
Film Tensile Strength at Break, TD 27.2 MPa3950 psiASTM D882
1% Secant Modulus, MD 134 MPa19400 psiASTM D882
1% Secant Modulus, TD 165 MPa23900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 4.5 %4.5 %ASTM D1003
Gloss 72 %72 %@ 45°. Base polymer; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °FWith blow-up ratios of 1.5:1 or higher.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8710 / 287821

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.