MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries. PVDF is also gaining recognition in automotive, building, electronics, food processing, pharmaceutical and battery applications. PVDF 11008/0001 combines excellent chemical resistance, dimensional stability and excellent flame and smoke resistance with a moderate degree of flexibility. (For applications requiring high degrees of flexibility, see our 30000 series copolymers.) PVDF 11008/0001 has set the standard for plenum rating jacketing and tubes, consistently achieving UL 150°C rating in numerous cable constructions and fiber raceway designs.

Features and Benefits:

  • PVDF 11008/0001 is a copolymer of VF2 and HFP (hexafluoropropylene)
  • Improved flexibility over PVDF homopolymers
  • Ideal for applications where high strength and a moderate degree of flexibility are required
  • Ideal for high speed extrusion
  • Excellent weatherability
  • Good chemical resistance
  • Long term use temperatures up to 150°C (302ºF)
  • Processable using most conventional thermoplastic conversion techniques
Information provided by Dyneon, A 3M Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.78 g/ccISO 1183
Water Absorption <= 0.040 %24 hr @ 23°C; ISO 62 (method 1)
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 24 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPa50mm/min; ASTM D638
Elongation at Break 600 %50mm/min; ASTM D638
Flexural Modulus 1.00 GPa2mm/min; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CCrystallinity by DSC; ASTM D3418
 
Descriptive Properties
FormGranules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride
Arkema KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion
Arkema Kynar Flex® 3120-10 PVDF
Arkema Kynar® UHM 6020-20 PVDF-GF

PDYNE066 / 34874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.