MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Safety-Walk™ 5100 Cushion Matting
Categories: Polymer

Material Notes: The product is a durable, flexible, vinyl mat having an open construction for easy, cleaning, comfort and safety. The mat has a low profile to minimize interference with foot and cart traffic. The vinyl composition offers excellent resistance to a variety of chemicals, greases and detergents found in industrial or food service environments.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 420 milASTM D418-68
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.20e+11 ohm-cm
Insulation Resistance 2.40e+11 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 60.0 °C
Minimum Service Temperature, Air -29.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carbon-Core CarbonFoam PU 2 R PU
Plutonium, Pu
Elektro-Isola Etronax MF G Phenolic, Cotton Fabric Reinforcement, Black, Sheets
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
Rogers Corporation R/bak® U Unsupported Cushion Mounting Material

PMM35277 / 170024

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.