MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sciengy PPS-SGRN101 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: PPS-SGRN101 is a linear polymer with high molecular weight, owns outstanding properties such as high temperature resistance, chemical and organic solvent resistance, non conducting, flame resistance, non-toxic, reliable performance and anti-adverse environment , with the strong bonding force of metal.

Applications: Based on the excellent properties, PPS Resin Coating grade can be used as coating material to make the inner/outer coating such as non-stick pan, machinery, chemical pipelines, reaction kettles and storage tanks etc.

Information provided by Shandong Sciengy New Materials Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.45 %
@Temperature 300 °C,
Time 3600 sec
The weight percentage of residue
Melt Flow 2500 g/10 min
@Load 5.00 kg,
Temperature 316 °C
2.095mm; ISO 1133
Ash <= 0.35 %ISO 3451
 
Descriptive Properties
Weight Loss<0.2%150?,1.0 hour,The weight percentage of the loss, ASTM D2288

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCIE065 / 297112

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.