System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Kinetics MIM F75 (ASTM F75) HIP
Categories:
Metal
;
Nonferrous Metal
;
Cobalt Alloy
;
Superalloy
;
Cobalt Base
Material Notes:
Most commonly used within the medical market on applications requiring these characteristics:
Bio-compatibility
Corrosion resistance
High strength
Nonmagnetic
Wear resistance.
Information provided by Kinetics, Inc.
Key Words:
Metal Injection Molding
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.25
g/cc
Sintered
Mechanical Properties
Original Value
Comments
Hardness, Rockwell C
25
Tensile Strength, Ultimate
>=
95.0
ksi
147
ksi
Typical
Tensile Strength, Yield
>=
65.0
ksi
81.0
ksi
Typical
Elongation at Break
>= 8.0 %
in 1 inch
30 %
in 1 inch Typical
Reduction of Area
40 %
Charpy Impact, Unnotched
130
ft-lb
1/2 size bar
Component Elements Properties
Original Value
Comments
Carbon, C
<= 0.15 %
Chromium, Cr
26 - 30 %
Cobalt, Co
58.85 - 68 %
Iron, Fe
<= 0.75 %
by difference
Manganese, Mn
<= 1.0 %
Molybdenum, Mo
5.0 - 7.0 %
Nickel, Ni
<= 1.0 %
Nitrogen, N
<= 0.25 %
Silicon, Si
1.0 %
Descriptive Properties
Surface Finish
40 Ra
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Arcam ASTM F-75 Cobalt Chrome Alloy
Carpenter BioDur™ CCM® Medical Implant Alloy, Annealed
Carpenter BioDur™ CCM® Medical Implant Alloy, Hot Worked
AISI Type 316L Stainless Steel, annealed and cold drawn bar
Carpenter BioDur™ CCM® Medical Implant Alloy, Warm Worked
NKINET14 / 138093
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.