System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Network Polymers Softflex® 4500
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Elastomer, Melt-Processible Rubber
Material Notes:
Description:
Softflex
®
Thermoplastic Elastomer Alloy
Information provided by Network Polymers Inc.
A. Schulman has acquired Network Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.18
g/cc
ASTM D792
Melt Flow
1.5
g/10 min
@Load 1.00 kg,
Temperature 235 °C
Procedure A Condition Q; ASTM D1238
11.5
g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore A
40 - 45
ASTM D792
Tensile Strength, Yield
600
psi
chs 20 in/min; ASTM D638
Elongation at Break
700 %
ASTM D638
Tear Strength
110
pli
ASTM D624
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Network Polymers Softflex® 0826
Network Polymers Softflex® 0809
Network Polymers Softflex® 0615
Network Polymers Softflex® 0470
Network Polymers Softflex® 0350
PDIAM013 / 29851
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.