MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil SAE 50 Mobilgard 570
Categories: Fluid; Lubricant

Material Notes: Mobilgard 570 by ExxonMobil is a superior quality, extra high performance, marine diesel engine cylinder oil. This bold new approach in cylinder lubricant technology provides maximum protection from adhesive and corrosive wear at the higher operating temperatures and pressures of todays modern crosshead engines. The outstanding performance of Mobilgard 570 has been demonstrated at the highest peak firing pressures and liner temperatures. Mobilgard 570 employs additives with substantially greater thermal stability and superior acid-corrosion protection. It has an optimum viscosity of over 20 cSt. at 100ºC and low volatility for best lubricant distribution and film retention. Through the use of unique formulation technology, the higher viscosity is attained with little or no use of thermally less stable, deposit-producing bright stock. Unique technology at the 70 TBN alkalinity level in Mobilgard 570 has demonstrated superior ring and liner protection and cleanliness under sustained operation with fuel sulphur levels down to 1.5%, but in some cases can be used in lower sulphur applications with the approval of the engine manufacturer.

Mobilgard 570 has been developed for marine crosshead engines designed for increased power and fuel efficiency. Such engines exhibit higher temperatures and pressures in the cylinder, which reduce the lubricants viscosity and increase the loads which it must withstand. Longer piston strokes have greatly increased the amount of surface to be protected and the amount of time the lubricant must withstand the severe cylinder temperatures and corrosive sulphur acids. Mobilgard 570 has also demonstrated superior performance in earlier engine designs. To ensure achieving the maximum equipment life possible, particular attention should be paid to the manufacturers special recommendations regarding the running-in of new rings and liners. Applications where the sulphur level is below 1.5% require special consideration and should be discussed with your ExxonMobil representative. Appropriate feed rates should be verified in all cases by through-the-ports inspection of liners for adequate oil film.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.937 g/cc
@Temperature 15.0 °C
Viscosity Measurement 104Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 229 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 21 cStASTM D445
 
Chemical PropertiesOriginal ValueComments
Total Base Number 70mgKOH/g; ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -9.00 °CASTM D97
Flash Point 256 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON337 / 75762

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.