MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Wellman Wellamid® XT1867-BK1 High Impact Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Description: High Impact Nylon 66

Information provided by Wellman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183-87
Linear Mold Shrinkage, Flow 0.025 - 0.030 cm/cm0.025 - 0.030 in/inISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.020 - 0.025 cm/cm0.020 - 0.025 in/inISO DIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiISO 527-93
Elongation at Break 140 %140 %ISO 527-93
Flexural Strength 55.0 MPa7980 psiISO 178-93
Flexural Modulus 1.45 GPa210 ksiISO 178-93
Izod Impact, Notched (ISO) 90.0 kJ/m²42.8 ft-lb/in²ISO 180-93
 22.0 kJ/m²
@Temperature -40.0 °C
10.5 ft-lb/in²
@Temperature -40.0 °F
ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FISO 75-93

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CP-Polymer-Technik Wellamid® 6600/58 HWCP Nylon 66, Impact Modified Until -40°C, Heat Stabilized, Dry
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Conditioned
CP-Polymer-Technik Wellamid® 6600/508 HWUVCP Nylon 66, Impact Modified, UV Stabilized, Heat Stabilized, Dry

PWEL739 / 72455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.