MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Adimoll® DB Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Adimoll® DB is a plasticizer for melt processable cellulose esters (CAB, CP), nitrocellulose, vinyl chloride-vinyl acetate copolymers (VCVAC), and polyvinyl chloride (PVC).

Chemical composition: Di-n-butyl adipate (DBA)

CAS reg. no.: 105-99-7

General Adimoll® DB is characterized by

  • good compatibility with cellulose derivates. It is used as low-temperature-resistant plasticizer for melt processable cellulose acetate butyrates and cellulose propionates.
  • very low viscosity, enabling the manufacture of highly filled pigment batches.
  • good compatibility with polyurethane systems
  • good gelling capacity for PVC but only a limited compatibility. Adimoll® DB can therefore only be added in small amounts to improve low-temperature resistance and reduce the viscosity of the plastisol.
  • high volatility and strong tendency to migrate; this property is very useful, for example, for plasticized PVC from which a constant migration of certain active ingredients over a prolonged period is desirable, e.g. in flea collars for dogs and cats.
  • a good compatibility with nitrocellulose.
Applications: Adimoll® DB is used as a plasticizer for a wide range of articles based on cellulose acetate butyrates and cellulose propionates, nitrocellulose and PVC. Typical fields of applications are calendering, extrusion, injection molding, pigment batches and carrier for active ingredients.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
Water Absorption <= 0.10 %<= 0.10 %DIN 51 777
Viscosity 6.0 cP6.0 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Pour Point -28.9 °C-20.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4351.435DIN EN ISO 6320
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Color<40Hazen, ISO 6271
Specifications116°CDissolution temperature, DIN 53408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8235 / 208628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.