MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond JL01 High Viscosity High Temperature Fiber Optic Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND JL01 is a high viscosity, two-component epoxy formulation that is suggested for bonding fiber optic bundles, potting glass fibers, and terminating single or multi-channel fiber optic connectors. The unique color change of this material ensures proper mixing and curing. TRA-BOND JL01 develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. It has good impact and thermal shock resistance, and yields excellent low stress, pot-and-polish connections that do not piston during cycle tests. It is also resistance to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 80000 cP
@Temperature 25.0 °C
80000 cP
@Temperature 77.0 °F
Mixed (rv #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 868630 min @ 150°C
Adhesive Bond Strength 26.2 MPa3800 psiLap shear, alum to alum, 15 min @ 100°C
 26.2 MPa3800 psiLap shear, alum to alum, 30 min @ 150°C
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 120 °C248 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 100 °C
0.250 hour
@Temperature 212 °F
 30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
Pot Life 40 min40 min
Working Life 90.0 min90.0 min
 
Descriptive Properties
Color BrownCured
Thixotropic Index 41 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC300 / 71228

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.