MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 108 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 108 is one of the most widely used plasticizers for nylon, other polyamides, shellac, cellulose acetate and protein materials.

Chemical composition: N-Ethyl o/p-toluene sulphonamide

General properties and Applications: Uniplex 108 is one of the most widely compatible plasticizers. It readily plasticizes nylon, other polyamides, shellac, cellulose acetate and protein materials. Uniplex 108 is outstanding for making compounds resistant to oils, solvents, and greases. For nylons, Uniplex 108 is one of the best plasticizers known. Uniplex 108 imparts toughness without adversely affecting other properties. It lowers the melting point and improves low temperature flexibility. In polyvinyl acetate adhesives, Uniplex 108’s good grease resistance and flexibility develops good tack for joining difficult surfaces, such as metal to rubber. In hot melts, Uniplex 108 improves flexibility for formulating book bindings and shoe adhesives. In cellulose acetate formulations, Uniplex 108 imparts excellent brilliance and gloss, while improving water and scuff resistance, oil resistance, and gives heat and light resistance to discoloration. In nitrocellulose lacquers, Uniplex 108 enhances adhesion, flexibility, and resistance to water, oils, and greases. Uniplex 108 is used when US regulations and recommendations governing food contacting applications need to be met. More information is available on request.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.185 g/cc
Viscosity 200 - 300 cP
 
Thermal PropertiesOriginal ValueComments
Boiling Point 196 °C
@Pressure 1.333 MPa
Pour Point 14.0 °F
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %Karl Fischer
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 0.010 %Inorganic Chloride
 
Descriptive Properties
AppearanceClear oily liquid
Color<200Hazen
Specifications<0.8%Acidity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Iran Petrochemical (PCC) EP-C 30 R Polypropylene
LyondellBasell Hostacom™ 6551 Polypropylene Homopolymer
Iran Petrochemical (PCC) C 30 S Polypropylene

PLANY9099 / 209490

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.