HTM140 High-Temperature mold material has a heat deflection temperature of 140°C straight out of the machine. High-definition parts printed in HTM140 can be directly vulcanized in rubber, eliminating the need for a metal master. It can be used in various applications that require thermal resistance, such as items to be metalized, high-temperature oil and gas applications or tools for small-run injection molding. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |