MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Krytox® XP 2A7 PFPE Grease
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE); PTFE Gellant

Material Notes: General information on the Krytox® XP line: Krytox® XP lubricants are high-quality, ultra-high-performance antifriction and antirust lubricants. Formulated with synthetic perfluoropolyether fluids, soluble additives, and efficient polytetrafluoroethylene thickeners, these lubricants exceed the performance requirements of most demanding applications.

Chemours was formed from former DuPont performance chemicals businesses, including DuPont Performance Lubricants, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 155Base Oil Viscosity Index
Kinematic Viscosity 1600 cSt
@Temperature 20.0 °C
Base Oil
Kinematic Viscosity at 40°C (104°F) 440 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 42 cStBase Oil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 288 °C
Minimum Service Temperature, Air <= -30.0 °C
Pour Point <= -30.0 °CBase Oil
 
Descriptive Properties
ISO Grade of Base Oil460

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Krytox® CORR 226 FG PFPE Corrugator Grease
Chemours Krytox® XHT-AC PFPE Grease
Chemours Krytox® XHT-BD Performance PFPE Lubricant
Chemours Krytox® XP 2A0 PFPE Grease
Chemours Krytox® XP 2A4 PFPE Grease

WDUPJ916 / 162450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.