MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade; LLDPE/Octene, Extruded; LLDPE/Hexene, Molded

Material Notes: Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.

Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low neck-in, excellent drawability and good gauge control. The combination of these features ensures films with outstanding optical properties and excellent impact and tear resistance.

Lumicene® mPE M 2735 S01 is suited for many applications in the field of cast film, stretch wrap film (low cling), hygiene film (f.e.. diaper backsheet), lamination and artificial grass.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.927 g/ccISO 1183
Thickness 20.0 microns
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 9.00 MPaISO 527-3
Film Tensile Strength at Yield, TD 9.00 MPaISO 527-3
Film Elongation at Break, MD 470 %ISO 527-3
Film Elongation at Break, TD 530 %ISO 527-3
Elmendorf Tear Strength, MD 5.10 g/micronISO 6383-2
Elmendorf Tear Strength, TD 12.2 g/micronISO 6383-2
Dart Drop Test 100 gISO 7765-1
Film Tensile Strength at Break, MD 39.0 MPaISO 527-3
Film Tensile Strength at Break, TD 24.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 119 °CISO 11357
Vicat Softening Point 118 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %ISO 14782
Gloss 89 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 - 60.0 °CChill Roll
Melt Temperature 240 - 280 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film
Total Lumicene® mPE M6040 S01 Metallocene Polyethylene, Cast Film
Total Lumicene® mPE M 5220 High Density Polyethylene, Blow Molding
Total Lumicene® mPE M 3509 Medium Density Polyethylene, Blow Molding
Total Lumicene® MR10MX0 Metallocene Random Copolymer Polypropylene, Injection Molding and Injection Blow Molding

PTOTAL774 / 130499

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.